Post-Processing and Finishing
Remove supports cleanly, sand, fill, prime and paint prints, add threaded inserts, smooth ABS, and wash and cure resin parts.
Welcome back!
Step 1 of 12Learn
From printer plate to finished object
A print straight off the machine is rarely the finished product. Post-processing can turn a layered, slightly rough part into something that looks injection molded, or simply make it functional.
Removing the part. Let the bed cool; many materials release on their own. Flex a spring-steel sheet to pop parts off. Avoid prying with sharp blades toward your hand. If you must use a scraper, push it away from yourself at a low angle.
Removing supports. Use flush cutters, needle-nose pliers and a deburring tool. Support interfaces and tree supports usually snap away; dense supports may need patient wiggling. Wear safety glasses, because small pieces of brittle support can fly. Cut, don't tear, near delicate features.
Cleaning up edges. A deburring tool shaves the sharp lip from edges and holes in one stroke. Lightly passing a heat gun or lighter over stray strings melts them away, but keep moving to avoid deforming the part. Holes can be drilled to exact size, and for a precise threaded hole you can tap threads directly into thick-walled PLA or PETG.
For strong, reusable threads, use heat-set inserts: small brass inserts pressed into a slightly undersized hole with a soldering iron. The plastic melts around their knurled surface, giving metal threads that survive many screw cycles, unlike threads printed or tapped in plastic.
Step 2 of 12Practice · Put in order
Order these steps for a painted display piece.
Drag the items, or use the arrow buttons, to put them in order.
- Apply color paint in thin coats
- Sand from coarse to fine grit
- Apply filler primer and sand again
- Finish with a clear protective coat
- Remove the part and its supports
Step 3 of 12Practice · Diagram
Sandpaper grit for printed parts
Which grit would you start with to flatten visible layer lines?
Tap the shape that answers the question, then press Check.
- 120
Coarse: removes layer lines and support scars quickly.
- 220
Removes the scratches left by 120 grit.
- 400
Good point to switch to wet sanding, especially with PLA.
- 800
Smooth surface ready for primer or paint.
- 1500
Very fine, for glossy clear coats or resin parts.
Step 4 of 12Learn
Sanding, filling, priming and painting
To hide layer lines on FDM parts:
- Sand progressively: start around 120–220 grit to flatten layer lines, then move to 400 and finer. Wet sanding (sandpaper and water) with the finer grits stops plastic from heating up and clogging the paper, which matters with PLA, which softens from friction heat.
- Fill deeper gaps with a spot putty or a thin layer of two-part filler, then sand again.
- Prime with a filler primer spray. It fills tiny scratches and layer lines and, because it's one even color, reveals defects you couldn't see before. Two or three rounds of priming and light sanding produce a very smooth surface.
- Paint with acrylics (brush or airbrush) or spray paint designed for plastic, in several thin coats rather than one thick one.
- Seal with a clear coat, matte or gloss, to protect the paint.
Choosing a smaller layer height reduces sanding work, and orienting the part so the most visible faces print vertically or face up helps too.
Other finishing options: epoxy coating, brushed on to fill lines and leave a glossy, hard shell; hydro-dipping for patterns; and vapor smoothing for ABS and ASA. In vapor smoothing, acetone vapor melts the outer surface into a glossy finish. Acetone is highly flammable and its vapor is harmful to breathe, so it's done only in small closed containers, outdoors or in strong ventilation, far from any heat or flame.
Step 5 of 12Practice · Fill in the blanks
Fill in the blanks
When sanding PLA, using water with fine-grit sandpaper is called . It keeps the plastic from softening due to friction .
Step 6 of 12Learn
Finishing resin prints
Resin parts come off the printer coated in sticky, uncured liquid and need two essential steps before they're safe to handle and fully strong.
- Wash. Rinse the part in isopropyl alcohol (IPA, 90% or stronger) or a resin-specific cleaner, usually in two baths: a "dirty" first bath and a cleaner second one. Wash stations stir the liquid automatically. Typical wash times are a few minutes; over-washing can make thin parts soft or cracked. Some "water-washable" resins rinse in water, but that water is still contaminated and must not go down the drain.
- Dry. Let the alcohol evaporate completely, or the next step can leave a white residue.
- Cure. Expose the part to UV light, in a curing station with a turntable or in sunlight, to fully harden it. Under-cured parts stay tacky and less strong; over-cured parts can become brittle and yellow.
Remove supports either before curing, when they snap off more easily, or after, when the part is stiffer. Then sand lightly (wet sanding is best, so no resin dust is created) and paint as with FDM parts.
Waste handling: used IPA contains dissolved resin. Leave it in a clear container in sunlight so the resin cures and settles, then dispose of the solid and liquid according to local hazardous-waste rules. Never pour it down the sink.
Step 7 of 12Diagram
Resin print from plate to finished part
Tap a shape with to see more.
- Remove from plate
Gloves on: the part is still covered in liquid resin.
- Wash in IPA
Two baths, a few minutes each; over-washing softens thin parts.
- Dry completely
Leftover alcohol leaves a white residue after curing.
- UV cure
Hardens the part fully; too much makes it brittle and yellow.
- Supports, sand, paint
Supports can come off before or after curing. Wet sand to avoid dust.
Step 8 of 12Note
Step 9 of 12Compare
Finishing FDM vs resin parts
| Aspect | FDM (filament) | Resin |
|---|---|---|
| Must-do steps | Remove part and supports | Wash, dry and UV cure |
| Main surface issue | Visible layer lines | Support marks; layers barely visible |
| Sanding | Coarse to fine; wet for PLA | Light, wet only, mask for dust |
| Safety focus | Hot nozzle, sharp tools, acetone vapor | Gloves until fully cured; resin waste |
Step 10 of 12Practice · Select all that apply
Which finishing methods suit a PLA cosplay helmet that must look smooth and painted? Select all that apply.
Select all that apply.
Step 11 of 12Practice · What would you do?
What would you do?
A maker wants a printed PETG enclosure lid to be screwed on and off dozens of times. What is the most durable approach for the screw holes?
Step 12 of 12Practice · True or false
Resin prints should be washed in alcohol or a suitable cleaner before UV curing.
Lesson complete!